ZnIn2Se4 is a ternary II-III-VI semiconductor compound combining zinc, indium, and selenium in a crystalline structure. This material belongs to the chalcogenide semiconductor family and is primarily investigated for optoelectronic and photovoltaic applications, where its direct bandgap and tunable electronic properties make it a candidate for light emission, detection, and energy conversion devices. While not yet widely commercialized, ZnIn2Se4 represents a research-stage compound with potential to address niche applications where conventional binary semiconductors (like ZnSe or InSe) fall short in terms of bandgap engineering or defect tolerance.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 34.98 | GPa | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.2800 | - | DFT · OptB88vdW | ||
Shear Modulus(G) | 20.25 | GPa | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 5.252 | kg/m³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)3 entries | 1.950 | eV | Measured | ||
| ↳ | 0.9320 | eV | DFT · OptB88vdW | ||
| ↳ | 2.246 | eV | DFT · TBmBJ | ||
Dielectric Constant (Relative Permittivity)(εr) | 12.63 | - | DFT · OptB88vdW | ||
High-Frequency Dielectric Constant (ε∞)(ε∞)2 entries | 9.034 | - | DFT · OptB88vdW | ||
| ↳ | 6.098 | - | DFT · TBmBJ | ||
Electron Effective Mass(m*e) | 0.1333 | me | DFT · OptB88vdW · 27°C | ||
Hole Effective Mass(m*h) | 0.7867 | me | DFT · OptB88vdW · 27°C | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW | ||
Piezoelectric Modulus(eij) | 0.5638 | C/m² | DFT · OptB88vdW | ||
Thermoelectric Power Factor(PF)2 entries | 0.000248 | W/(m·K²) | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 0.00284 | W/(m·K²) | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Seebeck Coefficient(S)2 entries | -46.99 | μV/K | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 302.3 | μV/K | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Spectroscopic Limited Maximum Efficiency (SLME)(SLME) | 17.76 | % | DFT · TBmBJ |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -0.5928 | eV/atom | DFT · OptB88vdW |