TaSbRu is an intermetallic ceramic compound combining tantalum, antimony, and ruthenium—a refractory material system designed for high-temperature and extreme-environment applications. This is an experimental or specialized composition rather than a commodity ceramic; materials in this family are investigated for aerospace, nuclear, and wear-resistant applications where conventional ceramics or superalloys reach their performance limits. The combination of heavy refractory elements suggests potential for thermal stability, hardness, and resistance to oxidation, making it relevant to engineers exploring next-generation materials for ultra-high-temperature structures or specialized coatings.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K)2 entries | 175.5 | GPa | DFT | ||
| ↳ | 177.6 | GPa | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.3300 | - | DFT · OptB88vdW | ||
Shear Modulus(G)2 entries | 70.26 | GPa | DFT | ||
| ↳ | 67.00 | GPa | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 11.29 | kg/m³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)2 entries | 0.8750 | eV | DFT · OptB88vdW | ||
| ↳ | 1.064 | eV | DFT · TBmBJ | ||
Dielectric Constant (Relative Permittivity)(εr)3 entries | 33.29 | - | DFT · OptB88vdW | ||
| ↳ | 32.43 | - | DFT · PBE | ||
| ↳ | 25.40 range 19.46–31.35median of 2 measurements | - | DFT · PBEsol | ||
High-Frequency Dielectric Constant (ε∞)(ε∞)2 entries | 20.95 | - | DFT · OptB88vdW | ||
| ↳ | 19.03 | - | DFT · TBmBJ | ||
Electronic Dielectric Tensor(ε∞) | Matrix (redacted) | - | DFT · PBE | ||
Total Dielectric Tensor(ε) | Matrix (redacted) | - | DFT · PBE | ||
Electron Effective Mass(m*e) | 0.4300 | me | DFT · OptB88vdW · 27°C | ||
Hole Effective Mass(m*h) | 0.6600 | me | DFT · OptB88vdW · 27°C | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW | ||
Piezoelectric Modulus(eij)2 entries | 0.5355 | C/m² | DFT · OptB88vdW | ||
| ↳ | 0.6707 | C/m² | DFT · PBE | ||
Piezoelectric Stress Tensor(eij) | Matrix (redacted) | C/m² | DFT · PBE | ||
Thermoelectric Power Factor(PF)2 entries | 0.00239 | W/(m·K²) | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 0.00399 | W/(m·K²) | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Seebeck Coefficient(S)2 entries | -200.7 | μV/K | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 321.3 | μV/K | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Spectroscopic Limited Maximum Efficiency (SLME)(SLME) | 32.37 | % | DFT · TBmBJ |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -0.3270 | eV/atom | DFT · OptB88vdW |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data