Sb₅IO₇ is an antimony iodine oxide semiconductor compound combining group 15 and halogen elements in a mixed-valence structure. This is a research-phase material primarily investigated for photocatalytic and optoelectronic applications, particularly in contexts where bismuth-free alternatives to traditional semiconductors are desirable. The material belongs to an emerging class of layered halide compounds being explored for visible-light photocatalysis, water treatment, and potentially thin-film electronic devices.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 5.555 | kg/m³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)3 entries | 1.950 | eV | Measured | ||
| ↳ | 2.460 | eV | DFT · OptB88vdW | ||
| ↳ | 3.497 | eV | DFT · TBmBJ | ||
Dielectric Constant (Relative Permittivity)(εr) | 16.43 | - | DFT · OptB88vdW | ||
High-Frequency Dielectric Constant (ε∞)(ε∞)2 entries | 5.694 | - | DFT · OptB88vdW | ||
| ↳ | 4.183 | - | DFT · TBmBJ | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW | ||
Piezoelectric Modulus(eij) | 0.1726 | C/m² | DFT · OptB88vdW | ||
Thermoelectric Power Factor(PF)2 entries | 0.00148 | W/(m·K²) | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 0.00165 | W/(m·K²) | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Seebeck Coefficient(S)2 entries | -209.7 | μV/K | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 289.5 | μV/K | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Spectroscopic Limited Maximum Efficiency (SLME)(SLME) | 1.310 | % | DFT · TBmBJ |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.01260 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -1.329 | eV/atom | DFT · OptB88vdW |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data