5086 Aluminum H36

Verifiedmetal

5086-H36 is a non-heat-treatable aluminum-magnesium alloy (approximately 3-4% Mg) commonly used in marine, pressure vessel, and aerospace applications requiring superior seawater corrosion resistance and weldability. The H36 temper (strain-hardened and partially annealed) provides moderate strength with enhanced formability compared to fully hard conditions, making it suitable for structural applications in sheet and plate form where both strength and corrosion resistance are critical.

aerospacestructural

Compliance & Regulations

?Conflict Free?FDA?RoHS?REACH?TSCA?Prop 65
5086 Aluminum/5086 Aluminum H36
Filter by
Form
e/D Ratio
Orientation
PropertyValueUnitConditionsSource
Ultimate Bearing Strength(Fbru)2 entries
ksi22°C · Sheet/Plate · H36 · AMS-QQ-A-250/7 · t=0.006-0.162 in · e/D=1.5
ksi22°C · Sheet/Plate · H36 · AMS-QQ-A-250/7 · t=0.006-0.162 in · e/D=2
Bearing Yield Strength(Fbry)
ksi22°C · Sheet/Plate · H36 · AMS-QQ-A-250/7 · t=0.006-0.162 in · e/D=1.5
Compressive Modulus(Ec)
ksi22°C · Sheet/Plate
Compressive Tangent Modulus vs Stress(Etn(σ))2 entries
Curve (11 pts)
ksi21°C · L
Curve (13 pts)
ksi21°C · LT
Compressive Yield Strength(Fcy)3 entries
ksi22°C · Sheet/Plate · H36 · AMS-QQ-A-250/7 · L · t=0.006-0.162 in
ksi22°C · Sheet/Plate · H36 · AMS-QQ-A-250/7 · LT · t=0.006-0.162 in
ksi22°C · Sheet/Plate · H36 · AMS-QQ-A-250/7 · ST · t=0.006-0.162 in
Poisson's Ratio(ν)
-22°C
Shear Modulus(G)
ksi22°C · Sheet/Plate
Ultimate Shear Strength(Fsu)
ksi22°C · Sheet/Plate · H36 · AMS-QQ-A-250/7 · t=0.006-0.162 in
Stress–Strain Curve (buckling region, ≤ 2% strain)(σ–ε (low-strain))4 entries
Curve (8 pts)
ksi21°C · L
Curve (11 pts)
ksi21°C · L
Curve (13 pts)
ksi21°C · LT
Curve (9 pts)
ksi21°C · LT
Ultimate Tensile Strength(σUTS)2 entries
ksi22°C · Sheet/Plate · H36 · AMS-QQ-A-250/7 · L · t=0.006-0.162 in
ksi22°C · Sheet/Plate · H36 · AMS-QQ-A-250/7 · LT · t=0.006-0.162 in
Yield Strength (0.2% offset)(σy)2 entries
ksi22°C · Sheet/Plate · H36 · AMS-QQ-A-250/7 · L · t=0.006-0.162 in
ksi22°C · Sheet/Plate · H36 · AMS-QQ-A-250/7 · LT · t=0.006-0.162 in
Young's Modulus(E)
ksi22°C · Sheet/Plate
N entriesMultiple entries per property — large groups are collapsed; click a summary row to expand. Use filters above to narrow by form / heat treatment / basis.
Rows with are inherited from the base material
Verified Unverified Low confidence (<80%) Link to source
PropertyValueUnitConditionsSource
CTE vs Temperature(α(T))
Curve (17 pts)
µin/in·°F
Thermal Conductivity vs Temperature(k(T))
Curve (20 pts)
BTU/(hr·ft·°F)
Rows with are inherited from the base material
Verified Unverified Low confidence (<80%) Link to source
PropertyValueUnitConditionsSource
Density(ρ)
lb/in³22°C
Rows with are inherited from the base material
Verified Unverified Low confidence (<80%) Link to source

Regulatory Screening

Environmental

Safety & Biocompatibility

Quality & Standards

Industry-Specific

RoHS, REACH, and Prop 65 statuses are validated against official substance lists (ECHA SVHC Candidate List, OEHHA Prop 65, RoHS Annex II). Other regulations are estimated from composition and material classification. All screening is a starting point for due diligence — always verify with your supplier before making compliance decisions.