Zn₂BiWO₆ is a complex oxide ceramic compound containing zinc, bismuth, and tungsten in a mixed-metal oxide structure. This material is primarily investigated in research contexts for photocatalytic and electronic applications, leveraging the semiconducting properties of bismuth and tungsten oxides combined with zinc's role in tuning bandgap and crystal structure. It represents an emerging class of multimetallic ceramics designed to improve photocatalytic efficiency under visible light, offering potential advantages over single-component oxide catalysts in environmental remediation and energy conversion applications.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.2985 | lb/in³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.000 | eV | DFT · OptB88vdW | ||
Magnetic Moment(μB) | 1.150 | µB | DFT · OptB88vdW | ||
Thermoelectric Power Factor(PF)2 entries | 0.000208 | W/(m·K²) | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 0.000189 | W/(m·K²) | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Seebeck Coefficient(S)2 entries | -17.35 | μV/K | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | -16.46 | μV/K | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.1602 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -1.690 | eV/atom | DFT · OptB88vdW |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data