Nickel-based superalloy (Ni-19.5Cr-13.5Co-4.3Mo-3Al-1.4Ti). 795 MPa yield, 1275 MPa UTS. Workhorse disc alloy for intermediate-temperature turbine stages (up to ~700°C). Good forgeability and weldability for a superalloy.
Compliance & Regulations
10 interactive curves for this material
Stress-strain, S-N fatigue and environmental knockdown curves are free with an account.
Create free account| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Elongation at Break(εf)2 entries | Curve (9 pts) | - | L | ||
| ↳ | Curve (8 pts) | - | L | ||
Ramberg–Osgood Exponent vs Temperature(n(T)) | Curve (10 pts) | - | — | ||
Reduction of Area vs Temperature(RA(T)) | Curve (10 pts) | - | L | ||
Stress–Strain Curve(σ–ε) | — | ksi | 5 entriesClick to expand | ||
Ultimate Tensile Strength(σUTS)2 entries | 184.9 | ksi | 20°C | ||
| ↳ | Curve (20 pts) | ksi | — | ||
Yield Strength (0.2% offset)(σy) | 115.3 | ksi | 20°C | ||
Young's Modulus(E)2 entries | 30,893 | ksi | — | ||
| ↳ | 30,600 | ksi | 22°C · Sheet/Strip/Plate | ||
3 interactive curves for this material
Stress-strain, S-N fatigue and environmental knockdown curves are free with an account.
Create free account| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
CTE vs Temperature(α(T)) | Curve (17 pts) | µin/in·°F | — | ||
Specific Heat vs Temperature(Cp(T)) | Curve (17 pts) | BTU/(lb·°F) | — | ||
Thermal Conductivity vs Temperature(k(T)) | Curve (17 pts) | BTU/(hr·ft·°F) | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ)2 entries | 0.2959 | lb/in³ | — | ||
| ↳ | 0.2980 | lb/in³ | 22°C |