TmHfIr2 is a ternary intermetallic ceramic compound combining thulium, hafnium, and iridium—a research-stage material belonging to the family of high-entropy and refractory intermetallics. This material is not yet established in mainstream industrial production but represents exploration into ultra-high-temperature ceramics and advanced structural compounds where extreme thermal stability, chemical inertness, and mechanical integrity are required. Engineers would consider this class of material for next-generation applications in aerospace propulsion, nuclear environments, or extreme-service applications where conventional ceramics and superalloys reach their limits.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 177.4 | GPa | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.5000 | - | DFT · OptB88vdW | ||
Shear Modulus(G) | 30.60 | GPa | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 16.57 | kg/m³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)2 entries | 0.000 | eV | DFT · OptB88vdW | ||
| ↳ | 0.000 | eV | DFT · TBmBJ | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW | ||
Thermoelectric Power Factor(PF)2 entries | 0.00214 | W/(m·K²) | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 0.00230 | W/(m·K²) | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Seebeck Coefficient(S)2 entries | -16.25 | μV/K | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | -16.90 | μV/K | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.04120 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -0.9776 | eV/atom | DFT · OptB88vdW |