Tl₃SbS₃ is a ternary thallium antimony sulfide ceramic compound belonging to the chalcogenide family, primarily of research interest rather than established commercial production. This material is investigated for potential applications in solid-state electronics and photonics due to its semiconducting properties and layered crystal structure, though it remains largely experimental with limited industrial deployment compared to more conventional semiconductors or optical ceramics. The compound represents an emerging area in materials research targeting niche applications in infrared optics and specialty electronic devices where its unique crystal chemistry may offer advantages over traditional alternatives.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 3,143 | ksi | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.3200 | - | DFT · OptB88vdW | ||
Shear Modulus(G) | 1,343 | ksi | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.2488 | lb/in³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)2 entries | 1.450 | eV | DFT · OptB88vdW | ||
| ↳ | 2.085 | eV | DFT · TBmBJ | ||
Dielectric Constant (Relative Permittivity)(εr)2 entries | 23.84 | - | DFT · OptB88vdW | ||
| ↳ | 21.36 | - | DFT · PBE | ||
High-Frequency Dielectric Constant (ε∞)(ε∞)2 entries | 10.63 | - | DFT · OptB88vdW | ||
| ↳ | 7.867 | - | DFT · TBmBJ | ||
Electronic Dielectric Tensor(ε∞) | Matrix (redacted) | - | DFT · PBE | ||
Total Dielectric Tensor(ε) | Matrix (redacted) | - | DFT · PBE | ||
Electron Effective Mass(m*e) | 0.7667 | me | DFT · OptB88vdW · 27°C | ||
Hole Effective Mass(m*h) | 1.227 | me | DFT · OptB88vdW · 27°C | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW | ||
Piezoelectric Modulus(eij) | 0.5145 | C/m² | DFT · OptB88vdW | ||
Thermoelectric Power Factor(PF)2 entries | 0.00295 | W/(m·K²) | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 0.00198 | W/(m·K²) | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Seebeck Coefficient(S)2 entries | -293.8 | μV/K | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 364 | μV/K | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Spectroscopic Limited Maximum Efficiency (SLME)(SLME) | 21.11 | % | DFT · TBmBJ |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -0.4059 | eV/atom | DFT · OptB88vdW |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data