Velo3D Ti-6Al-4V is that maker's grade of the alpha-beta titanium alloy made by laser powder bed fusion, here in the annealed condition. As built, rapid solidification gives columnar prior-beta grains along the build direction filled with fine acicular martensite, plus high residual stress and a rough surface. Annealing relieves the stress and turns the martensite into a fine alpha-beta structure with better ductility, though some anisotropy between build directions remains. Parts are typically machined on critical surfaces and may be hot isostatically pressed for fatigue-loaded service. They serve as lightweight aerospace brackets, ducts, manifolds and other complex titanium components. Every value on this page is read from Velo3D's own material data sheet — quoted, cited and dated — and is the maker's statement about printed material, not a measurement by MatWorld; none has yet been reviewed by a person.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Elongation at Break(εf) | 12.00 – 20.00 | % | 6 entriesClick to expand | ||
Ultimate Tensile Strength(σUTS) | 0.9500 – 1.045 | GPa | 6 entriesClick to expand | ||
Yield Strength (0.2% offset)(σy) | 775.0 – 891.0 | MPa | 6 entriesClick to expand | ||
Young's Modulus(E)2 entries | 107.0 range 101.0–113.0 | GPa | Grade 23 · annealed | ||
| ↳ | 107.5 range 103.0–112.0 | GPa | Grade 5 · annealed · Z | ||
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 4.429 | kg/m³ | 22°C |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data