EOS Titanium Ti64ELI in the heat-treated condition is the extra-low-interstitial Ti-6Al-4V (Grade 23) grade, processed by laser powder bed fusion and heat-treated after building. As built, rapid solidification gives fine acicular martensite within columnar prior-beta grains along the build direction, with high residual stress and limited ductility. Heat treatment relieves the stress and transforms the martensite into a fine lamellar alpha-beta structure, which improves ductility. Parts still need support removal and usually machining, and are used for orthopedic implants, lattice structures and lightweight aerospace components. Every value on this page is read from EOS's own material data sheet — quoted, cited and dated — and is the maker's statement about printed material, not a measurement by MatWorld; none has yet been reviewed by a person.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Elongation at Break(εf) | 8.700 – 14.00 | % | 6 entriesClick to expand | ||
Reduction of Area(RA)2 entries | 25.00 | % | minimum · heat-treated · EN ISO 6892-1 · Z | ||
| ↳ | 25.00 | % | minimum · heat-treated · EN ISO 6892-1 · XY | ||
Ultimate Tensile Strength(σUTS) | 150.8 – 184.2 | ksi | 6 entriesClick to expand | ||
Yield Strength (0.2% offset)(σy) | 134.9 – 159.5 | ksi | 6 entriesClick to expand | ||
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.1600 | lb/in³ | — | — |