TeAuI is an intermetallic compound combining tellurium, gold, and iodine, belonging to the family of ternary metal halides and chalcogenides. This is an experimental or specialized research material rather than a conventional structural alloy; such compounds are typically investigated for their unique electronic, optical, or thermoelectric properties that differ substantially from their constituent elements. TeAuI and related compositions show potential in semiconductor applications, energy conversion devices, and solid-state chemistry where the synergistic combination of these elements provides tailored functionality not achievable with binary systems.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 3,121.2 | ksi | — | ||
Poisson's Ratio(ν) | 0.3100 | - | — | ||
Shear Modulus(G) | 1,393.8 | ksi | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.2707 | lb/in³ | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.8520 | eV | — | ||
Magnetic Moment(μB) | 0.000 | µB | — | ||
Seebeck Coefficient(S) | -340.7 | µV/K | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | — | ||
Formation Energy(ΔHf) | -0.09946 | eV/atom | — |