Te9Mo8S7 is a ternary intermetallic compound combining tellurium, molybdenum, and sulfur. This is a research-phase material rather than a widely commercialized alloy; it belongs to the family of transition metal chalcogenides, which are studied for their potential in semiconducting, catalytic, and energy storage applications. The material's composition suggests interest in layered or complex crystal structures that could offer properties relevant to thermoelectric conversion, catalysis, or electronic devices where the combination of these three elements provides tunable electronic behavior.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.2259 | lb/in³ | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.8790 | eV | — | ||
Magnetic Moment(μB) | 0.000 | µB | — | ||
Seebeck Coefficient(S) | -325.7 | µV/K | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.03150 | eV/atom | — | ||
Formation Energy(ΔHf) | -0.5245 | eV/atom | — |