Te2Mo3WSe4S2
metalTe2Mo3WSe4S2 is a complex chalcogenide compound combining tellurium, molybdenum, tungsten, selenium, and sulfur—a multi-element metal chalcogenide material primarily explored in materials research rather than established industrial production. This composition sits at the intersection of semiconductor and metallurgical chemistry, with potential applications in thermoelectric energy conversion, photovoltaic devices, and advanced electronic systems where layered or mixed-valence transition metal chalcogenides offer tunable electronic and thermal properties. The material's utility depends on engineered crystal structure and doping; it represents an experimental platform for optimizing performance in niche high-tech applications where conventional alloys or single-element semiconductors fall short.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 34.98 | GPa | — | ||
Poisson's Ratio(ν) | 0.2200 | - | — | ||
Shear Modulus(G) | 23.79 | GPa | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 5.406 | kg/m³ | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.1590 | eV | — | ||
Dielectric Constant (Relative Permittivity)(εr) | 14.46 | - | — | ||
Magnetic Moment(μB) | 0.000 | µB | — | ||
Piezoelectric Modulus(eij) | 0.04067 | C/m² | — | ||
Seebeck Coefficient(S) | -24.73 | µV/K | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.1160 | eV/atom | — | ||
Formation Energy(ΔHf) | -0.5411 | eV/atom | — |