Tb2KCuS4 is an experimental ternary sulfide compound combining terbium, potassium, and copper in a mixed-metal sulfide framework. This material belongs to the family of rare-earth transition metal chalcogenides, which are primarily investigated in academic and research settings for their potential electronic, magnetic, and structural properties rather than established industrial production.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 8,420.9 | ksi | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.2600 | - | DFT · OptB88vdW | ||
Shear Modulus(G) | 4,950.1 | ksi | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.1801 | lb/in³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 1.010 | eV | DFT · OptB88vdW | ||
High-Frequency Dielectric Constant (ε∞)(ε∞) | 6.978 | - | DFT · OptB88vdW | ||
Electron Effective Mass(m*e) | 1.310 | me | DFT · OptB88vdW · 27°C | ||
Hole Effective Mass(m*h) | 1.933 | me | DFT · OptB88vdW · 27°C | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW | ||
Thermoelectric Power Factor(PF)2 entries | 0.00166 | W/(m·K²) | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 0.00121 | W/(m·K²) | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Seebeck Coefficient(S)2 entries | -190.9 | μV/K | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 251.7 | μV/K | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -1.810 | eV/atom | DFT · OptB88vdW |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data