SrLiP is an inorganic ceramic compound composed of strontium, lithium, and phosphorus. This material belongs to the class of phosphate-based ceramics and is primarily of research interest rather than an established commercial material. SrLiP and related strontium–lithium phosphate compositions are investigated for solid-state electrolyte and ion-conductor applications in advanced battery systems, as well as for bioceramics in bone-replacement and biomedical scaffolding due to strontium's bioactive properties. The combination of lithium (for ionic conductivity) and strontium (for biocompatibility and osteogenic activity) makes this compound potentially valuable in next-generation energy storage and regenerative medicine, though widespread industrial deployment remains limited.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K)2 entries | 44.30 | GPa | DFT | ||
| ↳ | 47.87 | GPa | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.1800 | - | DFT · OptB88vdW | ||
Shear Modulus(G)2 entries | 36.62 | GPa | DFT | ||
| ↳ | 39.54 | GPa | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 3.151 | kg/m³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)2 entries | 1.396 | eV | DFT · OptB88vdW | ||
| ↳ | 2.008 | eV | DFT · TBmBJ | ||
Dielectric Constant (Relative Permittivity)(εr)2 entries | 34.68 | - | DFT · OptB88vdW | ||
| ↳ | 13.94 range 8.159–19.71median of 2 measurements | - | DFT · PBEsol | ||
High-Frequency Dielectric Constant (ε∞)(ε∞)2 entries | 8.588 | - | DFT · OptB88vdW | ||
| ↳ | 6.931 | - | DFT · TBmBJ | ||
Electron Effective Mass(m*e) | 0.6500 | me | DFT · OptB88vdW · 27°C | ||
Hole Effective Mass(m*h) | 0.6833 | me | DFT · OptB88vdW · 27°C | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW | ||
Piezoelectric Modulus(eij)2 entries | 0.000 | C/m² | DFT · OptB88vdW | ||
| ↳ | 0.6202 | C/m² | DFT · PBE | ||
Piezoelectric Stress Tensor(eij) | Matrix (redacted) | C/m² | DFT · PBE | ||
Thermoelectric Power Factor(PF)2 entries | 0.00340 | W/(m·K²) | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 0.00190 | W/(m·K²) | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Seebeck Coefficient(S)2 entries | -262.6 | μV/K | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 213 | μV/K | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Spectroscopic Limited Maximum Efficiency (SLME)(SLME) | 22.80 | % | DFT · TBmBJ |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -1.111 | eV/atom | DFT · OptB88vdW |