Sr4I6O is an iodide-oxide ceramic compound containing strontium, representing an uncommon mixed-anion ceramic in the ternary Sr–I–O system. This material is primarily of academic and exploratory interest rather than established industrial production, with research focus on its crystal structure, ionic conductivity, and potential electrochemical properties characteristic of halide-oxide ceramics.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 4.858 | kg/m³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)2 entries | 4.042 | eV | DFT · OptB88vdW | ||
| ↳ | 5.030 | eV | DFT · TBmBJ | ||
Dielectric Constant (Relative Permittivity)(εr) | 9.812 | - | DFT · OptB88vdW | ||
High-Frequency Dielectric Constant (ε∞)(ε∞)2 entries | 4.452 | - | DFT · OptB88vdW | ||
| ↳ | 4.136 | - | DFT · TBmBJ | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW | ||
Piezoelectric Modulus(eij) | 0.04011 | C/m² | DFT · OptB88vdW | ||
Thermoelectric Power Factor(PF)2 entries | 0.000995 | W/(m·K²) | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 0.000645 | W/(m·K²) | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Seebeck Coefficient(S)2 entries | -303.6 | μV/K | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 325.5 | μV/K | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Spectroscopic Limited Maximum Efficiency (SLME)(SLME) | 0.000 | % | DFT · TBmBJ |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -2.053 | eV/atom | DFT · OptB88vdW |