SmSiRu is an intermetallic ceramic compound combining samarium, silicon, and ruthenium, belonging to the class of ternary transition metal silicides. This material is primarily of research and developmental interest, studied for applications requiring high-temperature structural performance and oxidation resistance due to the refractory nature of ruthenium-containing silicates and the thermal stability contributions of rare-earth samarium.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 14,470.4 | ksi | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.2900 | - | DFT · OptB88vdW | ||
Shear Modulus(G) | 7,675.4 | ksi | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.2784 | lb/in³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)2 entries | 0.000 | eV | DFT · OptB88vdW | ||
| ↳ | 0.000 | eV | DFT · TBmBJ | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW | ||
Thermoelectric Power Factor(PF)2 entries | 0.0000196 | W/(m·K²) | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 0.0000182 | W/(m·K²) | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Seebeck Coefficient(S)2 entries | 2.510 | μV/K | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 2.377 | μV/K | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -0.7436 | eV/atom | DFT · OptB88vdW |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data