ScTiO3 is a perovskite-structured ceramic compound combining scandium and titanium oxides. This material remains primarily a research-phase compound studied for its potential in high-temperature dielectric and ferroelectric applications, particularly where thermal stability and reduced loss tangent are desired compared to conventional titanate ceramics. The scandium-titanate family is of interest in microwave and RF device development, though industrial deployment remains limited compared to established titanate systems.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.1596 | lb/in³ | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)3 entries | 0.000 | eV | — | ||
| ↳ | 0.000 | eV | — | ||
| ↳ | 0.000 | eV | — | ||
Magnetic Moment(μB)3 entries | 0.01000 | μB | — | ||
| ↳ | -0.2754 | μB | — | ||
| ↳ | 3.885 | µB | — | ||
Seebeck Coefficient(S) | 31.90 | µV/K | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.08450 | eV/atom | — | ||
Formation Energy(ΔHf)3 entries | -2.894 | eV/atom | — | ||
| ↳ | 0.2600 | eV/atom | — | ||
| ↳ | -3.389 | eV/atom | — |