ScSnAu

metal
· ScSnAu

ScSnAu is a ternary intermetallic compound combining scandium, tin, and gold—a research-phase alloy belonging to the family of rare-earth and precious-metal intermetallics. This material is not yet established in mainstream engineering practice but represents an experimental composition of interest in materials science for exploring novel mechanical and physical properties that may arise from the combination of a light refractory metal (Sc), a common tin-based intermetallic former (Sn), and a noble metal (Au). Such ternary systems are typically investigated for fundamental studies of elastic behavior, phase stability, and potential applications in high-performance or specialized environments where conventional alloys fall short.

experimental intermetallic researchelastic properties characterizationhigh-temperature structural applications (potential)precious-metal alloy developmentaerospace materials screeningsemiconductor or optoelectronic device contexts (Au-bearing intermetallics)

Compliance & Regulations

?EAR?Conflict Free?RoHS?REACH?TSCA?Prop 65
PropertyValueUnitConditionsSource
Bulk Modulus(K)3 entries
11,918.7
ksi
13,051.9
ksi
12,658.9
ksi
Elastic Compliance Tensor(Sij)
Matrix (redacted)
1/GPa
Elastic Anisotropy(AU)
0.2522
-
Elastic Stiffness Tensor(Cij)
Matrix (redacted)
ksi
Poisson's Ratio(ν)2 entries
0.3029
-
0.3100
-
Shear Modulus(G)3 entries
5,408.5
ksi
6,184.3
ksi
5,298.2
ksi
N entriesMultiple entries per property — large groups are collapsed; click a summary row to expand. Use filters above to narrow by form / heat treatment / basis.
Verified Unverified Low confidence (<80%) Link to source
PropertyValueUnitConditionsSource
Density(ρ)
0.3322
lb/in³
Verified Unverified Low confidence (<80%) Link to source
PropertyValueUnitConditionsSource
Band Gap(Eg)
0.000
eV
Dielectric Constant (Relative Permittivity)(εr)2 entries
23.01
-
21.05
range 20.26–21.84median of 2 measurements
-
Electronic Dielectric Tensor(ε∞)
Matrix (redacted)
-
Total Dielectric Tensor(ε)
Matrix (redacted)
-
Magnetic Moment(μB)
0.000
µB
Piezoelectric Modulus(eij)
0.1992
C/m²
Piezoelectric Stress Tensor(eij)
Matrix (redacted)
C/m²
Seebeck Coefficient(S)
-24.06
µV/K
N entriesMultiple entries per property — large groups are collapsed; click a summary row to expand. Use filters above to narrow by form / heat treatment / basis.
Verified Unverified Low confidence (<80%) Link to source
PropertyValueUnitConditionsSource
Energy Above Hull(ΔEhull)
0.07840
eV/atom
Formation Energy(ΔHf)
-0.7033
eV/atom
Verified Unverified Low confidence (<80%) Link to source

Regulatory Screening

Environmental

Export Control

RoHS, REACH, and Prop 65 statuses are validated against official substance lists (ECHA SVHC Candidate List, OEHHA Prop 65, RoHS Annex II). Other regulations are estimated from composition and material classification. All screening is a starting point for due diligence — always verify with your supplier before making compliance decisions.