ScSbPt is a ternary intermetallic compound combining scandium, antimony, and platinum—a research-phase material belonging to the family of high-performance metallic systems. While not yet established in volume production, this compound is of interest to materials scientists exploring novel alloy combinations that leverage platinum's corrosion resistance and thermal stability alongside scandium's lightweight benefits and antimony's structural strengthening effects. Engineers and researchers investigating advanced aerospace, high-temperature structural, or specialized electronic applications would evaluate this material primarily for its potential elastic stiffness and density characteristics in demanding environments where conventional alloys reach performance limits.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K)2 entries | 15,940.3 | ksi | DFT | ||
| ↳ | 16,650.3 | ksi | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.3000 | - | DFT · OptB88vdW | ||
Shear Modulus(G)2 entries | 7,742.1 | ksi | DFT | ||
| ↳ | 7,588.4 | ksi | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.3334 | lb/in³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)2 entries | 0.5820 | eV | DFT · OptB88vdW | ||
| ↳ | 0.7480 | eV | DFT · TBmBJ | ||
Dielectric Constant (Relative Permittivity)(εr)3 entries | 23.12 | - | DFT · OptB88vdW | ||
| ↳ | 21.78 | - | DFT · PBE | ||
| ↳ | 19.91 range 18.68–21.15median of 2 measurements | - | DFT · PBEsol | ||
High-Frequency Dielectric Constant (ε∞)(ε∞)2 entries | 21.24 | - | DFT · OptB88vdW | ||
| ↳ | 17.48 | - | DFT · TBmBJ | ||
Electronic Dielectric Tensor(ε∞) | Matrix (redacted) | - | DFT · PBE | ||
Total Dielectric Tensor(ε) | Matrix (redacted) | - | DFT · PBE | ||
Electron Effective Mass(m*e) | 0.5600 | me | DFT · OptB88vdW · 27°C | ||
Hole Effective Mass(m*h) | 0.5700 | me | DFT · OptB88vdW · 27°C | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW | ||
Piezoelectric Modulus(eij)2 entries | 0.2676 | C/m² | DFT · OptB88vdW | ||
| ↳ | 0.1590 | C/m² | DFT · PBE | ||
Piezoelectric Stress Tensor(eij) | Matrix (redacted) | C/m² | DFT · PBE | ||
Thermoelectric Power Factor(PF)2 entries | 0.00283 | W/(m·K²) | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 0.00288 | W/(m·K²) | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Seebeck Coefficient(S)2 entries | -305.6 | μV/K | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 229.6 | μV/K | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Spectroscopic Limited Maximum Efficiency (SLME)(SLME) | 25.36 | % | DFT · TBmBJ |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -1.168 | eV/atom | DFT · OptB88vdW |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data