ScNiP is an intermetallic compound composed of scandium, nickel, and phosphorus, representing a research-phase material within the broader family of transition metal phosphides. This ternary system is primarily of academic and exploratory interest, with potential applications in high-performance functional materials where combination of mechanical stiffness, low density, and intermetallic strengthening mechanisms could offer advantages over conventional alloys.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K)2 entries | 21,984.6 | ksi | — | ||
| ↳ | 21,367 | ksi | — | ||
Poisson's Ratio(ν) | 0.2500 | - | — | ||
Shear Modulus(G)2 entries | 13,307.9 | ksi | — | ||
| ↳ | 12,764.8 | ksi | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.1909 | lb/in³ | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.000 | eV | — | ||
Dielectric Constant (Relative Permittivity)(εr)2 entries | 20.44 | - | — | ||
| ↳ | 18.31 range 16.57–20.05median of 2 measurements | - | — | ||
Magnetic Moment(μB) | 0.000 | µB | — | ||
Piezoelectric Modulus(eij) | 0.08952 | C/m² | — | ||
Seebeck Coefficient(S) | -70.24 | µV/K | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | — | ||
Formation Energy(ΔHf) | -1.227 | eV/atom | — |