ScIrO3 is a ternary oxide ceramic composed of scandium, iridium, and oxygen, belonging to the perovskite or perovskite-related oxide family. This is primarily a research material rather than a commodity ceramic; it is investigated for its potential as a functional oxide with applications in high-temperature electrochemistry, catalysis, and solid-state ionics, where the combination of scandium and iridium brings both ionic conductivity and chemical stability. ScIrO3 represents the broader class of mixed-metal oxides used to engineer materials for demanding thermal and electrochemical environments where conventional ceramics fall short.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.000 | eV | DFT · PBE | ||
Magnetic Moment(μB)2 entries | 0.000 | μB | DFT | ||
| ↳ | -0.0000175 | μB | DFT |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Formation Energy(ΔHf)2 entries | -1.303 | eV/atom | DFT | ||
| ↳ | 1.540 | eV/atom | DFT |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data