ScIr is an intermetallic ceramic compound combining scandium and iridium, representing a high-density refractory material from the transition-metal ceramics family. This material exhibits exceptional stiffness and thermal stability, making it candidates for extreme-environment applications where conventional ceramics or superalloys reach their performance limits. ScIr remains largely in the research and development phase, with potential applications in aerospace propulsion, wear-resistant coatings, and high-temperature structural components where its density and elastic properties provide advantages in demanding thermal and mechanical environments.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K)3 entries | 165.7 | GPa | — | ||
| ↳ | 165.7 | GPa | — | ||
| ↳ | 173.3 | GPa | — | ||
Elastic Compliance Tensor(Sij) | Matrix (redacted) | 1/GPa | — | ||
Elastic Anisotropy(AU) | 0.06628 | - | — | ||
Elastic Stiffness Tensor(Cij) | Matrix (redacted) | Pa | — | ||
Poisson's Ratio(ν)2 entries | 0.3025 | - | — | ||
| ↳ | 0.3600 | - | — | ||
Shear Modulus(G)3 entries | 75.36 | GPa | — | ||
| ↳ | 75.36 | GPa | — | ||
| ↳ | 61.10 | GPa | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 11.76 | kg/m³ | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)2 entries | 0.000 | eV | — | ||
| ↳ | 0.000 | eV | — | ||
Magnetic Moment(μB) | 0.000 | µB | — | ||
Seebeck Coefficient(S) | -3.590 | µV/K | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | — | ||
Formation Energy(ΔHf)2 entries | -0.9297 | eV/atom | — | ||
| ↳ | -1.137 | eV/atom | — |