ScBC is a scandium boron carbide ceramic compound combining scandium with boron and carbon phases to achieve high hardness and stiffness. This material family is primarily of research and developmental interest, explored for applications demanding extreme wear resistance and thermal stability where conventional ceramics may fall short. ScBC represents an emerging class of multi-element ceramics that can be engineered for specific mechanical and thermal properties, though industrial adoption remains limited compared to established boron carbide or silicon carbide alternatives.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 229.4 | GPa | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.1500 | - | DFT · OptB88vdW | ||
Shear Modulus(G) | 216.7 | GPa | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 4.177 | kg/m³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)2 entries | 0.000 | eV | DFT · OptB88vdW | ||
| ↳ | 0.000 | eV | DFT · TBmBJ | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.00630 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -0.6786 | eV/atom | DFT · OptB88vdW |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data