SbIrSe is a ternary intermetallic ceramic compound combining antimony, iridium, and selenium. This material belongs to the family of dense, high-modulus ceramics and is primarily encountered in materials research rather than established commercial production. The compound is of interest in thermoelectric and semiconductor applications where the combination of metallic elements with selenium provides potential for electronic or thermal transport properties, though SbIrSe remains largely an experimental material awaiting validation for engineering-scale deployment.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 128.3 | GPa | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.2500 | - | DFT · OptB88vdW | ||
Shear Modulus(G) | 79.00 | GPa | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 10.49 | kg/m³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)2 entries | 1.116 | eV | DFT · OptB88vdW | ||
| ↳ | 1.419 | eV | DFT · TBmBJ | ||
High-Frequency Dielectric Constant (ε∞)(ε∞) | 16.52 | - | DFT · TBmBJ | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW | ||
Spectroscopic Limited Maximum Efficiency (SLME)(SLME) | 33.43 | % | DFT · TBmBJ |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -0.4599 | eV/atom | DFT · OptB88vdW |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data