UltiMaker Nylon is UltiMaker's nylon filament grade for fused deposition modeling, which melts and extrudes it layer by layer into tough, slightly flexible parts. Like other printed nylons, the filament absorbs moisture readily and is dried and kept dry before printing to avoid bubbling, rough surfaces and weak layers. Parts are weaker across the layers than along them, show visible layer lines and tend to warp as they cool, so a heated bed, good bed adhesion and supports for overhangs are usually needed. Printed parts are used for functional prototypes, jigs and fixtures, snap fits, hinges and lightly loaded gears and wear parts. Every value on this page is read from UltiMaker's own material data sheet — quoted, cited and dated — and is the maker's statement about printed material, not a measurement by MatWorld; none has yet been reviewed by a person.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Notched Charpy Impact Strength(acN) | 13.70 range 12.50–14.90 | kJ/m² | 23°C · ISO 179-1 / 1eB · XY | ||
Elongation at Break(εf)3 entries | 120 | % | ASTM D3039 · XY | ||
| ↳ | 130 | % | YZ (Side) · ASTM D3039 | ||
| ↳ | 1.700 range 1.500–1.900 | % | ASTM D3039 · Z | ||
Flexural Modulus(Ef)3 entries | 1.872 range 1.782–1.962 | GPa | ISO 178 · XY | ||
| ↳ | 1.052 range 0.9960–1.108 | GPa | YZ (Side) · ISO 178 | ||
| ↳ | 1.060 range 1.002–1.118 | GPa | ISO 178 · Z | ||
Flexural Strength (MOR)(σf)3 entries | 82.90 range 79.80–86.00 | MPa | ISO 178 · XY | ||
| ↳ | 63.40 range 60.60–66.20 | MPa | YZ (Side) · ISO 178 | ||
| ↳ | 36.60 range 33.60–39.60 | MPa | ISO 178 · Z | ||
Hardness (Shore D)(Shore D) | 81.00 | Shore D | ISO 7619-1 · XY | ||
Ultimate Tensile Strength(σUTS)3 entries | 40.40 range 38.20–42.60 | MPa | ASTM D3039 · XY | ||
| ↳ | 42.30 range 41.00–43.60 | MPa | YZ (Side) · ASTM D3039 | ||
| ↳ | 23.00 range 20.70–25.30 | MPa | ASTM D3039 · Z | ||
Yield Strength (0.2% offset)(σy)2 entries | 63.10 range 62.00–64.20 | MPa | ASTM D3039 · XY | ||
| ↳ | 65.30 range 64.80–65.80 | MPa | YZ (Side) · ASTM D3039 | ||
Young's Modulus(E)3 entries | 2.331 range 2.276–2.386 | GPa | ASTM D3039 · XY | ||
| ↳ | 2.336 range 2.261–2.411 | GPa | YZ (Side) · ASTM D3039 | ||
| ↳ | 2.300 range 2.236–2.364 | GPa | ASTM D3039 · Z |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Glass Transition Temperature(Tg) | 328.3 | K | ISO 11357 | ||
Heat Deflection Temperature(HDT) | 362.4 range 356.8–368 | K | 0.45 MPa load · ISO 75-2 / B | ||
Melting Point / Solidus(Tm) | 461.6 | K | ISO 11357 | ||
Vicat Softening Temperature(VST) | 442.8 range 442–443.6 | K | ISO 306 / A120 |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 1.140 | kg/m³ | ISO 1183 |