NpAs is a ceramic compound composed of neptunium arsenide, belonging to the class of actinide pnictide ceramics. This material is primarily of research and academic interest rather than established industrial production, studied for its physical properties within the actinide materials science community. The compound represents a niche area of materials chemistry relevant to nuclear science, materials characterization under extreme conditions, and fundamental understanding of f-element ceramics.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 11,327.4 | ksi | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.2700 | - | DFT · OptB88vdW | ||
Shear Modulus(G) | 7,623.2 | ksi | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.3815 | lb/in³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)2 entries | 0.000 | eV | DFT · OptB88vdW | ||
| ↳ | 0.000 | eV | DFT · TBmBJ | ||
Magnetic Moment(μB) | 3.824 | µB | DFT · OptB88vdW | ||
Thermoelectric Power Factor(PF)2 entries | 0.000691 | W/(m·K²) | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 0.000697 | W/(m·K²) | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Seebeck Coefficient(S)2 entries | -33.76 | μV/K | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | -33.95 | μV/K | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -0.8769 | eV/atom | DFT · OptB88vdW |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data