NaSnP is an inorganic ceramic compound combining sodium, tin, and phosphorus elements, belonging to the family of metal phosphides and related ceramics. This material is primarily of research interest rather than established in widespread industrial production, with potential applications in solid-state chemistry, energy storage systems, and functional ceramic devices where tin phosphides have shown promise for electrochemical properties.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 0.000 | ksi | DFT · OptB88vdW | ||
Shear Modulus(G) | 0.000 | ksi | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.1335 | lb/in³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.5690 | eV | DFT · OptB88vdW | ||
Dielectric Constant (Relative Permittivity)(εr) | 16.31 | - | DFT · PBE | ||
High-Frequency Dielectric Constant (ε∞)(ε∞) | 11.59 | - | DFT · OptB88vdW | ||
Electronic Dielectric Tensor(ε∞) | Matrix (redacted) | - | DFT · PBE | ||
Total Dielectric Tensor(ε) | Matrix (redacted) | - | DFT · PBE | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW | ||
Piezoelectric Modulus(eij) | 0.2994 | C/m² | DFT · PBE | ||
Piezoelectric Stress Tensor(eij) | Matrix (redacted) | C/m² | DFT · PBE |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -0.3672 | eV/atom | DFT · OptB88vdW |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data