Mo5As4 is a molybdenum arsenide intermetallic compound belonging to the family of metal-arsenide phases, characterized by a defined stoichiometric structure rather than a solid solution. This material is primarily of research and exploratory interest rather than established in high-volume production; molybdenum arsenides are investigated for their potential in thermoelectric applications, catalysis (particularly hydrogen evolution), and high-temperature structural applications where the combination of refractory metal properties and intermetallic strengthening could provide advantages over pure molybdenum or conventional alloys.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 21,973.2 | ksi | — | ||
Poisson's Ratio(ν) | 0.2700 | - | — | ||
Shear Modulus(G) | 12,287.6 | ksi | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.3014 | lb/in³ | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)2 entries | 0.000 | eV | — | ||
| ↳ | 0.000 | eV | — | ||
Magnetic Moment(μB) | 0.000 | µB | — | ||
Seebeck Coefficient(S) | -0.7600 | µV/K | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | — | ||
Formation Energy(ΔHf) | -0.2366 | eV/atom | — |