MgTe₂ is a magnesium telluride ceramic compound belonging to the family of II-VI semiconducting ceramics. This material remains primarily in the research and development phase rather than established industrial production, with investigation focused on its potential as a wide-bandgap semiconductor and thermoelectric material. MgTe₂ is of interest in advanced optoelectronics, thermal management systems, and high-temperature device applications where its ceramic stability and electronic properties could offer advantages over conventional semiconductors, though its brittleness and processing challenges limit current practical deployment.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K)2 entries | 5,474.8 | ksi | DFT | ||
| ↳ | 5,907.4 | ksi | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.2500 | - | DFT · OptB88vdW | ||
Shear Modulus(G)2 entries | 3,143 | ksi | DFT | ||
| ↳ | 3,475.1 | ksi | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.1889 | lb/in³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)2 entries | 1.100 | eV | DFT · OptB88vdW | ||
| ↳ | 1.728 | eV | DFT · TBmBJ | ||
Dielectric Constant (Relative Permittivity)(εr) | 14.77 | - | DFT · PBE | ||
High-Frequency Dielectric Constant (ε∞)(ε∞)2 entries | 11.04 | - | DFT · OptB88vdW | ||
| ↳ | 8.146 | - | DFT · TBmBJ | ||
Electronic Dielectric Tensor(ε∞) | Matrix (redacted) | - | DFT · PBE | ||
Total Dielectric Tensor(ε) | Matrix (redacted) | - | DFT · PBE | ||
Electron Effective Mass(m*e) | 0.6000 | me | DFT · OptB88vdW · 27°C | ||
Hole Effective Mass(m*h) | 0.5900 | me | DFT · OptB88vdW · 27°C | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW | ||
Thermoelectric Power Factor(PF)2 entries | 0.000894 | W/(m·K²) | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 0.00356 | W/(m·K²) | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Seebeck Coefficient(S)2 entries | -232.4 | μV/K | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 279.6 | μV/K | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Spectroscopic Limited Maximum Efficiency (SLME)(SLME) | 28.79 | % | DFT · TBmBJ |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -0.6362 | eV/atom | DFT · OptB88vdW |