LuBiO3 is a rare-earth bismuth oxide ceramic compound combining lutetium (the heaviest stable lanthanide) with bismuth oxide. This material belongs to the family of complex rare-earth oxides and is primarily of research interest rather than established industrial production, with potential applications in photonic and electronic materials where high density and rare-earth properties provide functional advantages.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.3459 | lb/in³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)3 entries | 2.498 | eV | DFT · OptB88vdW | ||
| ↳ | 3.957 | eV | DFT · TBmBJ | ||
| ↳ | 0.000 | eV | DFT · PBE | ||
High-Frequency Dielectric Constant (ε∞)(ε∞)2 entries | 5.688 | - | DFT · OptB88vdW | ||
| ↳ | 4.258 | - | DFT · TBmBJ | ||
Magnetic Moment(μB)2 entries | 0.000 | μB | DFT | ||
| ↳ | 0.000 | µB | DFT · OptB88vdW | ||
Spectroscopic Limited Maximum Efficiency (SLME)(SLME) | 0.04000 | % | DFT · TBmBJ |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.05370 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf)2 entries | -1.379 | eV/atom | DFT | ||
| ↳ | -2.610 | eV/atom | DFT · OptB88vdW |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data