LiAuO2 is an oxide ceramic compound containing lithium and gold, belonging to the mixed-metal oxide family. This material is primarily of research and development interest rather than established in high-volume industrial production, with potential applications in advanced ceramics, electronic materials, and specialized functional applications where the unique properties of gold-doped lithium oxides may offer advantages. Engineers would consider this material for niche applications requiring the specific thermal, electrical, or chemical properties that the lithium-gold oxide system provides, though availability and cost considerations typically limit its use to specialized research and prototype development rather than commodity engineering applications.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 15,668.4 | ksi | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.3800 | - | DFT · OptB88vdW | ||
Shear Modulus(G) | 5,346.1 | ksi | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.2965 | lb/in³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)2 entries | 1.704 | eV | DFT · OptB88vdW | ||
| ↳ | 1.719 | eV | DFT · TBmBJ | ||
Dielectric Constant (Relative Permittivity)(εr)2 entries | 11.35 | - | DFT · OptB88vdW | ||
| ↳ | 7.581 range 6.140–9.022median of 2 measurements | - | DFT · PBEsol | ||
High-Frequency Dielectric Constant (ε∞)(ε∞)2 entries | 7.094 | - | DFT · OptB88vdW | ||
| ↳ | 6.443 | - | DFT · TBmBJ | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW | ||
Piezoelectric Modulus(eij) | 0.1641 | C/m² | DFT · OptB88vdW | ||
Thermoelectric Power Factor(PF)2 entries | 0.00271 | W/(m·K²) | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 0.000596 | W/(m·K²) | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Seebeck Coefficient(S)2 entries | -344.5 | μV/K | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 452.8 | μV/K | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Spectroscopic Limited Maximum Efficiency (SLME)(SLME) | 28.90 | % | DFT · TBmBJ |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -1.050 | eV/atom | DFT · OptB88vdW |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data