K4ZnP2 is an inorganic ceramic compound composed of potassium, zinc, and phosphorus elements, belonging to the phosphide ceramic family. This material is primarily of research and developmental interest rather than established in mainstream industrial production, with potential applications in solid-state chemistry and functional ceramics where mixed-metal phosphides offer unique electronic or ionic properties. Engineers investigating this compound would typically be exploring advanced ceramics for specialized applications requiring low density combined with moderate stiffness, such as in emerging electronic, photonic, or thermal management systems where conventional oxides or nitrides may be unsuitable.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 2,744.1 | ksi | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.3000 | - | DFT · OptB88vdW | ||
Shear Modulus(G) | 1,446 | ksi | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.07182 | lb/in³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)2 entries | 1.018 | eV | DFT · OptB88vdW | ||
| ↳ | 2.503 | eV | DFT · TBmBJ | ||
Dielectric Constant (Relative Permittivity)(εr)3 entries | 10.91 | - | DFT · OptB88vdW | ||
| ↳ | 8.630 | - | DFT · PBE | ||
| ↳ | 6.634 range 4.741–8.527median of 2 measurements | - | DFT · PBEsol | ||
High-Frequency Dielectric Constant (ε∞)(ε∞)2 entries | 5.825 | - | DFT · OptB88vdW | ||
| ↳ | 3.355 | - | DFT · TBmBJ | ||
Electronic Dielectric Tensor(ε∞) | Matrix (redacted) | - | DFT · PBE | ||
Total Dielectric Tensor(ε) | Matrix (redacted) | - | DFT · PBE | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW | ||
Piezoelectric Modulus(eij) | 0.000 | C/m² | DFT · OptB88vdW | ||
Thermoelectric Power Factor(PF)2 entries | 0.000567 | W/(m·K²) | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 0.000793 | W/(m·K²) | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Seebeck Coefficient(S)2 entries | -82.72 | μV/K | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 403.5 | μV/K | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Spectroscopic Limited Maximum Efficiency (SLME)(SLME) | 12.58 | % | DFT · TBmBJ |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -0.5040 | eV/atom | DFT · OptB88vdW |