K4Te6U2 is an experimental intermetallic semiconductor compound combining potassium, tellurium, and uranium in a defined stoichiometric ratio. This material belongs to the family of uranium-based chalcogenides and represents a research-phase compound rather than an established commercial material; its semiconducting properties and mixed-metal composition suggest potential relevance to advanced electronic, thermoelectric, or nuclear materials research where uranium-bearing compounds are systematically evaluated for specialized applications.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 3,532.5 | ksi | — | ||
Shear Modulus(G) | 2,264.5 | ksi | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.00600 | eV | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Formation Energy(ΔHf) | -1.018 | eV/atom | — |