HS 188 Solution Treated

Verifiedmetal

HS 188 is a cobalt-based superalloy with tungsten and chromium additions, designed for high-temperature structural applications in gas turbines and aerospace engines requiring sustained performance above 1000°C. Solution-treated condition provides optimal balance of strength and ductility through controlled heat treatment, suitable for sheet applications where creep resistance and thermal fatigue resistance are critical performance requirements.

aerospacestructural

Compliance & Regulations

?EAR?Conflict Free?RoHS?REACH?TSCA?Prop 65
HS 188/HS 188 Solution Treated
Filter by
Thickness
Orientation
PropertyValueUnitConditionsSource
Compressive Modulus(Ec)
ksi22°C · Sheet
Compressive Yield Strength(Fcy)2 entries
ksi22°C · Sheet · Solution Treated · AMS 5608 · LT · t=<0.020 in
ksi22°C · Sheet · Solution Treated · AMS 5608 · LT · t=0.020-0.187 in
Elongation at Break(εf)2 entries
-22°C · Sheet · Solution Treated · AMS 5608 · LT · t=<0.020 in
-22°C · Sheet · Solution Treated · AMS 5608 · LT · t=0.020-0.187 in
Poisson's Ratio(ν)
-22°C
Shear Modulus(G)
ksi22°C · Sheet
Ultimate Shear Strength(Fsu)2 entries
ksi22°C · Sheet · Solution Treated · AMS 5608 · t=<0.020 in
ksi22°C · Sheet · Solution Treated · AMS 5608 · t=0.020-0.187 in
Ultimate Tensile Strength(σUTS)4 entries
ksi22°C · Sheet · Solution Treated · AMS 5608 · L · t=<0.020 in
ksi22°C · Sheet · Solution Treated · AMS 5608 · L · t=0.020-0.187 in
ksi22°C · Sheet · Solution Treated · AMS 5608 · LT · t=<0.020 in
ksi22°C · Sheet · Solution Treated · AMS 5608 · LT · t=0.020-0.187 in
Yield Strength (0.2% offset)(σy)4 entries
ksi22°C · Sheet · Solution Treated · AMS 5608 · L · t=<0.020 in
ksi22°C · Sheet · Solution Treated · AMS 5608 · L · t=0.020-0.187 in
ksi22°C · Sheet · Solution Treated · AMS 5608 · LT · t=<0.020 in
ksi22°C · Sheet · Solution Treated · AMS 5608 · LT · t=0.020-0.187 in
Young's Modulus(E)
ksi22°C · Sheet
N entriesMultiple entries per property — large groups are collapsed; click a summary row to expand. Use filters above to narrow by form / heat treatment / basis.
Rows with are inherited from the base material
Verified Unverified Low confidence (<80%) Link to source
PropertyValueUnitConditionsSource
CTE vs Temperature(α(T))
Curve (18 pts)
µin/in·°F
Specific Heat vs Temperature(Cp(T))
Curve (18 pts)
BTU/(lb·°F)
Thermal Conductivity vs Temperature(k(T))
Curve (18 pts)
BTU/(hr·ft·°F)
Rows with are inherited from the base material
Verified Unverified Low confidence (<80%) Link to source
PropertyValueUnitConditionsSource
Density(ρ)
lb/in³22°C
Rows with are inherited from the base material
Verified Unverified Low confidence (<80%) Link to source

Regulatory Screening

Environmental

Export Control

RoHS, REACH, and Prop 65 statuses are validated against official substance lists (ECHA SVHC Candidate List, OEHHA Prop 65, RoHS Annex II). Other regulations are estimated from composition and material classification. All screening is a starting point for due diligence — always verify with your supplier before making compliance decisions.