HoSbPd is an intermetallic ceramic compound containing holmium, antimony, and palladium, representing an experimental material from the rare-earth intermetallic family. This compound has been primarily studied in materials research contexts for its potential in high-performance applications requiring specific combinations of mechanical stiffness and damping behavior. While not yet established in commercial production, intermetallic compounds of this type are being investigated for applications demanding thermal stability, corrosion resistance, or specialized electromagnetic properties in demanding environments.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 11,012.7 | ksi | — | ||
Poisson's Ratio(ν) | 0.4900 | - | — | ||
Shear Modulus(G) | 359.7 | ksi | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.3130 | lb/in³ | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.4340 | eV | — | ||
Dielectric Constant (Relative Permittivity)(εr) | 21.53 | - | — | ||
Magnetic Moment(μB) | 0.000 | µB | — | ||
Piezoelectric Modulus(eij) | 0.4014 | C/m² | — | ||
Seebeck Coefficient(S) | -255.2 | µV/K | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.2663 | eV/atom | — | ||
Formation Energy(ΔHf) | -0.7046 | eV/atom | — |