Ge2N2O is an oxynitride ceramic compound combining germanium, nitrogen, and oxygen elements, representing a mixed-valence ceramic system. This material belongs to the broader family of advanced oxynitride ceramics, which are primarily of research and development interest rather than established commercial commodities. The compound's potential applications lie in high-temperature structural applications, electronic ceramics, or specialized optical coatings where the unique combination of germanium bonding with nitrogen and oxygen phases could provide distinctive mechanical or functional properties compared to single-phase alternatives.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 14,405.1 | ksi | — | ||
Poisson's Ratio(ν) | 0.2400 | - | — | ||
Shear Modulus(G) | 8,889.4 | ksi | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.1691 | lb/in³ | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 2.363 | eV | — | ||
Dielectric Constant (Relative Permittivity)(εr)3 entries | 7.730 | - | — | ||
| ↳ | 8.775 | - | — | ||
| ↳ | 5.887 range 4.147–7.627median of 2 measurements | - | — | ||
Electronic Dielectric Tensor(ε∞) | Matrix (redacted) | - | — | ||
Total Dielectric Tensor(ε) | Matrix (redacted) | - | — | ||
Magnetic Moment(μB) | 0.000 | µB | — | ||
Piezoelectric Modulus(eij)2 entries | 0.2254 | C/m² | — | ||
| ↳ | 0.6884 | C/m² | — | ||
Piezoelectric Stress Tensor(eij) | Matrix (redacted) | C/m² | — | ||
Seebeck Coefficient(S) | -89.12 | µV/K | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.07960 | eV/atom | — | ||
Formation Energy(ΔHf) | -0.5169 | eV/atom | — |