GaSiMo4S8 is a quaternary compound combining gallium, silicon, molybdenum, and sulfur—a rare composition that does not correspond to established commercial alloys or well-documented industrial materials. This appears to be an experimental or research-phase compound, likely investigated for semiconducting, photovoltaic, or chalcogenide-based electronic properties given its sulfide chemistry and mixed-metal framework. Engineers should treat this as an emerging material whose performance, manufacturability, and long-term stability remain under investigation; it is not recommended for production applications without extensive characterization and validation.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 43.40 | GPa | — | ||
Shear Modulus(G) | -9.720 | GPa | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 4.181 | kg/m³ | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.2050 range 0.000–0.4100median of 2 measurements | eV | — | ||
Dielectric Constant (Relative Permittivity)(εr) | 23.96 | - | — | ||
Magnetic Moment(μB) | 0.000 | µB | — | ||
Piezoelectric Modulus(eij) | 0.1767 | C/m² | — | ||
Seebeck Coefficient(S) | -19.42 | µV/K | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.3754 | eV/atom | — | ||
Formation Energy(ΔHf) | -0.4829 | eV/atom | — |