GaNiRh₂ is a ternary intermetallic compound combining gallium, nickel, and rhodium, representing a research-phase material within the family of high-performance metallic intermetallics. This compound belongs to the broader class of transition-metal-based alloys that are typically investigated for applications requiring exceptional mechanical stability and thermal resistance at elevated temperatures. While not yet in mainstream commercial production, materials in this composition family are explored for their potential in aerospace, catalytic, and high-temperature structural applications where conventional nickel-based superalloys or rhodium-containing catalysts may have limitations.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 29,336.8 | ksi | — | ||
Poisson's Ratio(ν) | 0.3700 | - | — | ||
Shear Modulus(G) | 11,153.4 | ksi | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.3767 | lb/in³ | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.000 | eV | — | ||
Magnetic Moment(μB) | 1.559 | µB | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.00640 | eV/atom | — | ||
Formation Energy(ΔHf) | -0.3045 | eV/atom | — |