CuBi2Se4O12 is a mixed-metal oxide ceramic compound containing copper, bismuth, selenium, and oxygen. This is a research-phase material, likely investigated for its potential electronic, thermal, or photocatalytic properties given its complex multi-element composition; it belongs to the family of chalcogenide and bismuth-based ceramics that have attracted academic interest for semiconducting and energy applications. Industrial adoption remains limited, but such materials are studied as candidates for thermoelectric devices, photocatalysts, or specialized optical components where the combination of heavy elements and mixed valence states can enable novel functionality.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 5.562 | kg/m³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.6740 | eV | DFT · OptB88vdW | ||
High-Frequency Dielectric Constant (ε∞)(ε∞) | 5.538 | - | DFT · OptB88vdW | ||
Magnetic Moment(μB) | 1.994 | µB | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -0.9931 | eV/atom | DFT · OptB88vdW |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data