CrAuO2 is an experimental ceramic compound combining chromium, gold, and oxygen phases, representing a research-stage material in the mixed-metal oxide family. While not yet established in mainstream engineering applications, this material is of interest in specialized research contexts involving noble-metal oxide ceramics, potentially for applications requiring unique thermal, electrical, or catalytic properties. Engineers should note this remains largely in development; industrial adoption and long-term performance data are limited compared to conventional ceramic alternatives.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.3456 | lb/in³ | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.6620 | eV | — | ||
Dielectric Constant (Relative Permittivity)(εr) | 15.97 | - | — | ||
Magnetic Moment(μB) | 6.000 | µB | — | ||
Piezoelectric Modulus(eij) | 0.000 | C/m² | — | ||
Seebeck Coefficient(S) | -284 | µV/K | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.1748 | eV/atom | — | ||
Formation Energy(ΔHf) | -1.409 | eV/atom | — |