CaZrBe is an experimental intermetallic compound combining calcium, zirconium, and beryllium. This material belongs to the family of lightweight refractory metals and intermetallics, currently in research and development phase rather than established industrial production. The combination of these elements targets applications requiring low density with moderate stiffness, though practical use remains limited due to beryllium's toxicity concerns, manufacturing challenges, and the material's relative immaturity in the engineering market compared to conventional titanium or aluminum alloys.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 54.84 | GPa | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.2400 | - | DFT · OptB88vdW | ||
Shear Modulus(G) | 34.47 | GPa | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 3.542 | kg/m³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.08600 | eV | DFT · OptB88vdW | ||
High-Frequency Dielectric Constant (ε∞)(ε∞) | 58.83 | - | DFT · OptB88vdW | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW | ||
Thermoelectric Power Factor(PF)2 entries | 0.000112 | W/(m·K²) | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 0.000193 | W/(m·K²) | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Seebeck Coefficient(S)2 entries | -31.21 | μV/K | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 10.33 | μV/K | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.2767 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | 0.1750 | eV/atom | DFT · OptB88vdW |