Bi83Sb17 is a bismuth-antimony intermetallic compound, a brittle ceramic material belonging to the group of bismuth-based compounds with potential thermoelectric applications. This composition sits within the bismuth-antimony phase diagram and is primarily of research interest for thermoelectric energy conversion and thermal management in specialized applications where the bismuth-antimony system's unique electronic and thermal transport properties offer advantages over conventional alternatives.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Electrical Conductivity(σ)2 entries | 3,506.5 | S/cm | 127°C | ||
| ↳ | 3,852.7 | S/cm | 27°C | ||
Electrical Resistivity(ρe)2 entries | 0.00000285 | Ω·m | 127°C | ||
| ↳ | 0.00000260 | Ω·m | 27°C | ||
Thermoelectric Power Factor(PF)2 entries | 0.00133 | W/(m·K²) | 127°C | ||
| ↳ | 0.00218 | W/(m·K²) | 27°C | ||
Seebeck Coefficient(S)2 entries | -61.60 | μV/K | 127°C | ||
| ↳ | -75.20 | μV/K | 27°C |