BeGaTe is a ternary ceramic compound composed of beryllium, gallium, and tellurium elements, belonging to the class of semiconducting or optoelectronic ceramics. This material is primarily of research and development interest rather than established high-volume industrial use, with potential applications in specialized optoelectronic and photonic devices where the unique electronic properties of the beryllium-gallium-tellurium system offer advantages over conventional III-V semiconductors or alternative wide-bandgap materials.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 6,008.9 | ksi | — | ||
Poisson's Ratio(ν) | 0.1400 | - | — | ||
Shear Modulus(G) | 261.1 | ksi | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.1723 | lb/in³ | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.000 | eV | — | ||
Magnetic Moment(μB) | 0.000 | µB | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.6236 | eV/atom | — | ||
Formation Energy(ΔHf) | 0.3416 | eV/atom | — |