BeCr4W is a complex beryllium-chromium-tungsten alloy that combines the lightweight properties of beryllium with the high-temperature strength and hardness of chromium and tungsten. This material is primarily of research and specialized industrial interest, valued in applications requiring the exceptional strength-to-weight ratio that beryllium alloys provide, particularly where thermal stability and wear resistance are critical and beryllium's unique advantages justify its cost and processing complexity.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.3269 | lb/in³ | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.000 | eV | — | ||
Magnetic Moment(μB) | 0.000 | µB | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.2120 | eV/atom | — | ||