BaNaP is a ceramic compound composed of barium, sodium, and phosphorus elements, representing a phosphate-based ceramic material. This material falls within the family of mixed-metal phosphate ceramics, which are primarily of research and development interest for specialized applications requiring chemically stable, non-metallic matrices. The material's potential applications span solid-state chemistry, ion-conducting systems, and advanced ceramic matrices where thermal stability and low chemical reactivity are advantageous; however, as an emerging compound, it remains less established in high-volume industrial production compared to conventional phosphate ceramics like calcium phosphates or aluminum phosphates.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 1,431.5 | ksi | — | ||
Poisson's Ratio(ν) | -0.06000 | - | — | ||
Shear Modulus(G) | 542.4 | ksi | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.1339 | lb/in³ | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.8640 | eV | — | ||
Dielectric Constant (Relative Permittivity)(εr)3 entries | 21.10 | - | — | ||
| ↳ | 21.49 | - | — | ||
| ↳ | 14.57 range 8.810–20.33median of 2 measurements | - | — | ||
Electronic Dielectric Tensor(ε∞) | Matrix (redacted) | - | — | ||
Total Dielectric Tensor(ε) | Matrix (redacted) | - | — | ||
Magnetic Moment(μB) | 0.000 | µB | — | ||
Piezoelectric Modulus(eij)2 entries | 0.02103 | C/m² | — | ||
| ↳ | 0.1791 | C/m² | — | ||
Piezoelectric Stress Tensor(eij) | Matrix (redacted) | C/m² | — | ||
Seebeck Coefficient(S) | -129.7 | µV/K | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | — | ||
Formation Energy(ΔHf) | -0.8992 | eV/atom | — |