Ba3ZnN2O is an experimental oxynitride ceramic compound combining barium, zinc, nitrogen, and oxygen in a complex ceramic structure. This material belongs to the family of mixed-anion ceramics (oxynitrides), which are primarily of research interest for their potential to bridge properties between traditional oxides and nitrides. While not yet in widespread industrial production, oxynitride ceramics like Ba3ZnN2O are being investigated for advanced applications requiring combinations of hardness, thermal stability, and ionic conductivity that conventional single-anion ceramics cannot easily achieve.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 9,399.9 | ksi | — | ||
Poisson's Ratio(ν) | 0.2900 | - | — | ||
Shear Modulus(G) | 4,793.5 | ksi | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.1992 | lb/in³ | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.6520 | eV | — | ||
Magnetic Moment(μB) | 0.000 | µB | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | — | ||
Formation Energy(ΔHf) | -1.231 | eV/atom | — |