AZ31B H26
VerifiedmetalAZ31B is a wrought magnesium alloy containing aluminum and zinc, widely used in aerospace and automotive applications where light weight and moderate strength are required. The H26 temper (strain-hardened and partially annealed) provides intermediate strength and ductility suitable for sheet and plate applications, with good formability and improved corrosion resistance compared to softer tempers.
aerospacestructural
Compliance & Regulations
?EAR?Conflict Free?RoHS?REACH?TSCA?Prop 65
Filter by
Form
Thickness
e/D Ratio
Orientation
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Ultimate Bearing Strength(Fbru) | — | Pa | 6 entriesClick to expand | ||
Bearing Yield Strength(Fbry) | — | Pa | 6 entriesClick to expand | ||
Compressive Modulus(Ec) | — | Pa | 22°C · Sheet | — | |
Compressive Tangent Modulus vs Stress(Etn(σ)) | Curve (12 pts) | Pa | 21°C · L | — | |
Compressive Yield Strength(Fcy) | — | Pa | 7 entriesClick to expand | ||
Elongation at Break(εf) | — | - | 7 entriesClick to expand | ||
Poisson's Ratio(ν) | — | - | 22°C | — | |
Shear Modulus(G) | — | Pa | 22°C · Sheet | — | |
Ultimate Shear Strength(Fsu)3 entries | — | Pa | 22°C · Plate · H26 · AMS 4376 · t=0.250-0.375 in | — | |
| ↳ | — | Pa | 22°C · Plate · H26 · AMS 4376 · t=0.376-0.438 in | — | |
| ↳ | — | Pa | 22°C · Plate · H26 · AMS 4376 · t=0.439-0.500 in | — | |
S–N Curve (Wöhler)(S–N) | Curve (40 pts) | Pa | 21°C · LT | — | |
Stress–Strain Curve (buckling region, ≤ 2% strain)(σ–ε (low-strain)) | Curve (8 pts) | Pa | 21°C · L | — | |
Ultimate Tensile Strength(σUTS) | — | Pa | 14 entriesClick to expand | ||
Yield Strength (0.2% offset)(σy) | — | Pa | 14 entriesClick to expand | ||
Young's Modulus(E) | — | Pa | 22°C · Sheet | — | |
N entriesMultiple entries per property — large groups are collapsed; click a summary row to expand. Use filters above to narrow by form / heat treatment / basis.
Rows with are inherited from the base material
Verified Unverified Low confidence (<80%) Link to source
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
CTE vs Temperature(α(T)) | Curve (7 pts) | 1/K | — | — | |
Thermal Conductivity vs Temperature(k(T)) | Curve (6 pts) | W/(m·K) | — | — |
Rows with are inherited from the base material
Verified Unverified Low confidence (<80%) Link to source
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | — | kg/m³ | 22°C | — |
Rows with are inherited from the base material
Verified Unverified Low confidence (<80%) Link to source
Regulatory Screening
Environmental
Export Control
RoHS, REACH, and Prop 65 statuses are validated against official substance lists (ECHA SVHC Candidate List, OEHHA Prop 65, RoHS Annex II). Other regulations are estimated from composition and material classification. All screening is a starting point for due diligence — always verify with your supplier before making compliance decisions.