As₃W₂ is an intermetallic compound combining arsenic and tungsten, representing a brittle metallic phase that forms in the As-W binary system. This material is primarily of research and industrial interest in high-temperature applications and specialized alloy development, where its thermal stability and density make it relevant for refractory or wear-resistant compositions. Engineers may encounter As₃W₂ as a constituent phase in tungsten-based alloys or in studies of heavy-metal intermetallics, though direct engineering use remains limited compared to conventional tungsten alloys or superalloys.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 19,729.5 | ksi | — | ||
Poisson's Ratio(ν) | 0.2600 | - | — | ||
Shear Modulus(G) | 12,052.6 | ksi | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.3966 | lb/in³ | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.000 | eV | — | ||
Magnetic Moment(μB) | 0.000 | µB | — | ||
Seebeck Coefficient(S) | 10.28 | µV/K | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.1700 | eV/atom | — | ||
Formation Energy(ΔHf) | -0.05277 | eV/atom | — |