AlTeI7 is an intermetallic compound combining aluminum, tellurium, and iodine; this is a research-phase material not yet widely commercialized. The compound belongs to the family of halide-containing intermetallics, which are being investigated for potential applications in solid-state electronics, layered heterostructures, and energy storage systems where layered crystal structures and tunable electronic properties are advantageous.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 1,380.8 | ksi | DFT · OptB88vdW | ||
Exfoliation Energy(Eexf) | 95.51 | meV/atom | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.3200 | - | DFT · OptB88vdW | ||
Shear Modulus(G) | 665.7 | ksi | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.1547 | lb/in³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 1.774 | eV | DFT · OptB88vdW | ||
Dielectric Constant (Relative Permittivity)(εr) | 11.16 | - | DFT · OptB88vdW | ||
High-Frequency Dielectric Constant (ε∞)(ε∞) | 7.063 | - | DFT · OptB88vdW | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW | ||
Piezoelectric Modulus(eij) | 0.1355 | C/m² | DFT · OptB88vdW | ||
Thermoelectric Power Factor(PF)2 entries | 0.000246 | W/(m·K²) | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 0.000551 | W/(m·K²) | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Seebeck Coefficient(S)2 entries | -344.1 | μV/K | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 313.4 | μV/K | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -0.3567 | eV/atom | DFT · OptB88vdW |